Technical Documentation
Material Safety DataSheet 7N171 EN
Material Safety DataSheet 7N171 1013 EN
Material Safety DataSheet 7N171 9005 EN
Technical DataSheet 7N170 EN
Material Safety DataSheet 7N171 EN
Material Safety DataSheet 7N171 1013 EN
Material Safety DataSheet 7N171 9005 EN
Material Safety DataSheet 7N172 9980 EN
Technical DataSheet 7N175 EN
Material Safety DataSheet 7N171 EN
Material Safety DataSheet 7N171 1013 EN
Material Safety DataSheet 7N171 9005 EN
Material Safety DataSheet 7N176 9980 EN
Interested in this product?

We are at your disposal, do not hesitate in contacting us.

Contacts

Preparation and Application

Steel: blast clean the steel to Sa 2½ grade, according to ISO 8501-1. The roughness profile should be adjusted, depending on the thickness of the product to be applied. Remove powder residues and abrasive residues from surface. These indications are generic, applicable to several products and merely informative.

Concrete: the concrete should be allowed to have a minimum 28 days to harden, a minimal tensile strength of 1.5 N/mm² and a minimum compression resistance of 25 N/mm². The surface must be clean, dry, free from laitance, old paints and other contaminants.

Aluminium: remove oil, grease or soap film with neutral detergent or emulsion cleaner. Blast lightly with fine abrasive.

Galvanized Surfaces: remove any oil soap film using a neutral detergent. Treat the surface in accordance with a lightly blast with fine abrasive. If galvanizing has been exposed to exterior weathering for 6 months or more, remove zinc corrosion products by mechanical means, like power sander. Remove oil grease with the cleaner.

For more information see the Technical DataSheet or contact us.